EFFECT OF COLD WORK ON HAZ WELD DECAY OF TYPE AISI 304 STAINLESS STEEL
DOI:
https://doi.org/10.66411/jer.v15i.228الكلمات المفتاحية:
Cold work، Type AISI304 stainless steel، Weld decay، electrochemical potentiokinetic reactivationالملخص
The weld decay (sensitization) of type 304 stainless steel (SS) is evaluated as a function of prior cold work and welding heat input. Type AISI 304SS is cold rolled to various percentages of thickness reduction up to 50% cold reduction (CR) at ambient temperature before being TIG welded. The susceptibility of 304SS to weld decay is evaluated using ASTM A262 practice A and electrochemical potentiokinetic reactivation (EPR) tests.
The results indicate that the influence of pre-welding cold work on the degree of sensitization (DOS) appears to be distinct and appreciable within the range of 10% to 35%CR. In addition within this range the critical level of cold work after which the DOS starts decreasing is found to be inversely related to the amount of welding heat input. Meanwhile, at higher levels of deformation approximately ≥ 35CR%, the results indicate that neither the cold work nor the welding heat input significantly influences the amount of DOS. Analysis of the reactivation scans obtained after the EPR test demonstrate that the DOS is almost independent of the activation current density (Ia), rather the reactivation current density (Ir) mostly influences the results. Microstructural investigation shows that the priority of the intergranular corrosion (IGC) appears to be at austenite grain boundaries and less likely at ferrite / austenite interfaces of the weld metal. Meanwhile, transgranular attack at austenite bulk matrix along the defects is rarely observed.
المراجع
[1] Murr L. E., Advani A. H., Shankar S., and Atteridge D.G., Materials Characterization, 24, 1990, p. 135. DOI: https://doi.org/10.1016/1044-5803(90)90032-F
[2] Trillo E. A., Beltran R., Maldonado J.G., Romero R. J., Murr L. E., Fisher W. W. and Advani A. H., Materials Characterization, 35, 1995, p. 99. DOI: https://doi.org/10.1016/1044-5803(95)00072-0
[3] Briant C. L. and Ritter A. M., Corrosion, 38, 1982, p.596 DOI: https://doi.org/10.5006/1.3578208
[4] Pednekar S., and Smialowska S., Corrosion, 36, 1980, p. 565. DOI: https://doi.org/10.5006/0010-9312-36.10.565
[5] Tedmon J. R., Vermilyea D. A., and Brocker D. E., Corrosion, 47, 1971, p.104. DOI: https://doi.org/10.5006/0010-9312-27.3.104
[6] Annual Book of ASTM Standards, ASTM, Philadelphia, PA, 03.02, 1990.
[7] Akashi M., T., Kawamoto F., and Umemura G. B, Corrosion Engineering, 29, 1980, p.163. DOI: https://doi.org/10.3323/jcorr1974.29.4_163
[8] Mayuzumi M., Ohta J., and Arai T., Corrosion, 54, 1998, p.27 DOI: https://doi.org/10.5006/1.3284853
[9] Parvathavarthini N., Dayal R. k., Seshadri S.K., and Gnanmoorthy J. B., Br. Corr. J, 1991, p.67. DOI: https://doi.org/10.1179/000705991798269332
[10] Raghuvir Singh B., Ravikumar A., Deykumar P. K., and Chattoraj I., Metall, Mat. Trans, 34A, 2002, P.2441 DOI: https://doi.org/10.1007/s11661-003-0004-5
[11] Brüemmer S M., Charlot L. A., and Atteridge D.G., Corrosion, 44, 1988, P. 427. DOI: https://doi.org/10.5006/1.3583958
[12] Bain E. C., Aborn R. H. and Rutherford J. B., Trans. Amer. Soc. Steel Treating, 21, 1933, p.481
[13] Garcia C., Martin F., Tiedra P. De, Heredero J. A., and Aparicio M. L., Corrosion, 56, 2000, p.243. DOI: https://doi.org/10.5006/1.3287650
التنزيلات
منشور
إصدار
القسم
الرخصة
الحقوق الفكرية (c) 2011 مجلة البحوث الهندسية (ليبيا)

هذا العمل مرخص بموجب Creative Commons Attribution 4.0 International License.