ACOUSTIC EMISSION OBSERVATION OF ULTIMATE ELASTIC WALL STRESS (UEWS) TEST UNDER PURE HYDROSTATIC PRESSURE FOR GLASS REINFORC ED EPOXY PIPE (GRE) PIPES

المؤلفون

  • Tarak Assaleh Mechanical Engineering, Faculty of Engineering, Sabratah University المؤلف
  • Asya A. Gabbasa Mechanical Engineering, Faculty of Engineering, Zawia University المؤلف
  • Siddig Dabbashi Mechanical Engineering, Faculty of Engineering, Sabratah University المؤلف

DOI:

https://doi.org/10.66411/jer.v25i.324

الكلمات المفتاحية:

Debonding Acoustic Emission، Ultimate Elastic Wall Stress، Matrix Cracks

الملخص

This paper presents the Acoustic Emission (AE) observations made for enhancing the ultimate elastic wall stress (UEWS) results for ±55° fiberglass reinforced pipes. The acoustic emissions tests were implemented under pure hydrostatic pressure. The AE measurement of pure hydrostatic pressure showed that matrix cracks were initiated early in the tests and delamination failure has occurred before the UEWS point. Significant AE events were only noticed when buckling induced delamination and debonding failure, which was followed by fibre fracture at the outer surface of the pipe.

212 90

المراجع

[1] Ramirez, G., M.D. Engelhardt, and T.J. Fowler, “On the endurance limit of fiberglass pipes using acoustic emission” . Journal of Pressure Vessel Technology, Transactions of the ASME, 2006, 128 (3): p.p. 454-461.

[2] Benmedakhene, S., M. Kenane, and M.L. Benzeggagh, “Initiation and growth of delamination in glass/epoxy composites subjected to static and dynamic loading by acoustic emission monitoring” . Composites Science and Technology, 1999, 59 (2): p.p. 201-208. DOI: https://doi.org/10.1016/S0266-3538(98)00063-3

[3] Dogossy, G. and T. Czigány, “Failure mode characterization in maize hull filled polyethylene composites by acoustic emission” . Polymer Testing, 2006. 25 (3): p.p. 353-357. DOI: https://doi.org/10.1016/j.polymertesting.2005.12.004

[4] Ramirez, G., M.D. Engelhardt, and T.J. Fowler, “On the Endurance Limit of Fiberglass Pipes Using Acoustic Emission” . Journal of Pressure Vessel Technology, 2006, 128 (3): p.p. 454-461. DOI: https://doi.org/10.1115/1.2218351

[5] Finkenstadt, V.L., C.-K. Liu, and R. Evangelista, “Poly (lactic acid) green composites using oilseed coproducts as fillers” . Industrial Crops and Products, 2007. 26(1): p.p. 36-43. DOI: https://doi.org/10.1016/j.indcrop.2007.01.003

[6] Khalifa AB, Zidi M, Abdelwahed L.” Mechanical characterization of glass/vinylester ±55° filament wound pipes by acoustic emission under axial monotonic loading” . C.R. Mec. 2012, 340: p.p. 453–460 DOI: https://doi.org/10.1016/j.crme.2012.02.006

التنزيلات

منشور

30-03-2018

إصدار

القسم

المقالات

كيفية الاقتباس

[1]
T. Assaleh, A. A. Gabbasa, و S. Dabbashi, "ACOUSTIC EMISSION OBSERVATION OF ULTIMATE ELASTIC WALL STRESS (UEWS) TEST UNDER PURE HYDROSTATIC PRESSURE FOR GLASS REINFORC ED EPOXY PIPE (GRE) PIPES", JER, م 25, ص 9–18, مارس 2018, doi: 10.66411/jer.v25i.324.